APPLICATION OF LASER SURFACE POLISHING ON ADDITIVE MANUFACTURED PARTS OF INCONEL 718 NICKEL-BASED SUPERALLOY

Abstract

This article deals with the influence of laser polishing parameters on the final surface quality of nickel-based superalloy Inconel 718 produced by metal additive manufacturing. The aim is to optimize the laser polishing process parameters to reduce the surface roughness of the sample. The investigated parameters of the laser are scanning speed, frequency, focal length, and pulsed and continuous wave regimes are considered. The samples of Inconel 718 are produced by direct metal laser sintering technology. Depending on the printing orientation, the roughness after AM is Ra 5 – 12 μm. The samples were machined to ensure uniformity of the monitored and tested surface. An IFM – G4 3D optical microscope is used for the surface evaluation. The initial roughness of the samples before applying laser polishing was Ra 1 - 2 μm. The roughness after laser polishing is significantly reduced to Ra 0.369 μm.

Recommended articles

DESIGN OF TEST RIGS FOR MEASURING DYNAMIC PROPERTIES OF SOFT ACTUATORS

Alexander Hosovsky, Monika Trojanova
Keywords: Soft Actuators | Fluid Muscle | Dielectric Elastomer Actuator (DE) | Ionic Polymer Metal Composites Actuator (IPMC) | Nonlinear Dynamic Characteristic

EXPERIMENTAL SETUP FOR ANALYZING FUNDAMENTALS OF CUTTING PROCESSES USING A MODULAR SYSTEM

Jim A. Bergmann, Rafael Garcia Carballo, Petra Wiederkehr, Jonas Baumann, Florian Wöste
Keywords: orthogonal cutting | oblique cutting | process dynamics | cutting fundamentals | modular experimental setup